Support

JKMG & International,
The Company that value for its customers
Support

Technical Support | (Trouble Shooting) Rust

JKMG         0       1,091   22-04-04 14:25

본문

 

  • Rust

    PhenomenonCoated film is partially swollen or peeled off by the rust of the substrate under the film.
    CauseA. Improper preparation of the substrate.
    B. Coating on the moisture.
    C. Water in the air hose.
    D. Low adhesion or rust resistance of the product.
    RepairRemove the damaged part on the substrate and apply the anti rust coating before the top coat.
    (Washprimer (DNU-800) + Primer-surfacer)
    PreventionA. Remove the moisture completely before applying.
    B. Prepare the substrate according to the standard.
    C. Apply the primer before the top coat.

 

JKMG & International can be contacted at : jessie.kim@jkmg-int.com Copyright © JKMG & INTERNATIONAL Co Inc. All rights reserved.